System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Marex Composites Mycell M040 PVC Foam Core
Categories:
Other Engineering Material
;
Composite Core Material
;
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Foam Grade
Material Notes:
Mycell is a PVC structural foam material that Marex Composites customizes for standard finishes from Maricell in Italy.
Property data reported are nominal/average values.
Information provided by Marex Composites.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.0400
g/cc
ISO 845
Water Absorption
1.0 %
Mechanical Properties
Original Value
Comments
Tensile Strength
0.710
MPa
ASTM D1623
Elongation at Break
9.0 %
Shear elongation; ISO 1922
Tensile Modulus
27.0
MPa
ASTM D1623
Compressive Strength
0.460
MPa
ISO 844
Compressive Modulus
36.0
MPa
ISO 844
Shear Modulus
0.0120
GPa
ASTM C393
Shear Strength
0.460
MPa
ASTM C393
Thermal Properties
Original Value
Comments
Thermal Conductivity
0.0310
W/m-K
ISO 8301
Descriptive Properties
Color
Azure
Fire Resistance
DIN5510 S4 SR2 ST2 FED<1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for PVC, Foam Grade
CoreLite BoardĀ® Closed-Cell PVC Foam
CoreLite PVC 80 Closed-Cell PVC Foam Sheet
DIAB KlegecellĀ® R 45 Rigid, Closed Cell PVC Foam Core Material
CoreLite PVC 60 Closed-Cell PVC Foam Sheet
PMAREX970 / 230566
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.