MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Telles Mirel™ P5001 Film Grade PHA Bioplastic  (discontinued **)
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Mirel P5001 is a high biobased content film grade with a high melt strength designed for blown and cast film extrusion. It is heat sealable and has excellent tensile properties, good puncture toughness, and tear propagation resistance. BPI certified to ASTM D6400 and Vincotte certified to EN 13432 standards for compostable plastics.

About Mirel Bioplastics

Mirel is a family of bioplastic materials that have physical properties comparable to petroleum-based resins, yet are both biobased and biodegradable in natural soil and water environments, home composting systems, and industrial composting facilities, where these facilities are available. The rate and extent of Mirel's biodegradablility will depend on the size and shape of the articles made from it. However, like nearly all bioplastics and organic matter, Mirel is not designed to biodegrade in conventional landfills.

Example applications include retail carry bags; yard waste/kitchen compost bags for use in home or commercial composting facilities;anaerobic digestion where facilities are available; and for agricultural films where biodegradability in soil is a primary benefit.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Polyhydroxyalkanoate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Bulk Density 0.720 g/ccpellets
Water Vapor Transmission 124 g/m²/dayASTM F1249
Oxygen Transmission 140 cc-mil/100 in²-24hr-atmASTM D3985
Viscosity 950 cP
@Shear Rate 100 1/s,
Temperature 180 °C
Apparent melt viscosity; 5 sec dwell time; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 404 %ASTM D882
Film Elongation at Break, TD 463 %ASTM D882
Secant Modulus, MD 0.300 GPaASTM D882
Secant Modulus, TD 0.320 GPaASTM D882
Elmendorf Tear Strength, MD 200 g/milASTM D1922
Elmendorf Tear Strength, TD 603 g/milASTM D1922
Dart Drop 150 g/milASTM D1709
Film Tensile Strength at Break, MD 20.0 MPaASTM D882
Film Tensile Strength at Break, TD 20.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °C
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648-07
Vicat Softening Point 119 °CASTM D1525-09
 
Optical PropertiesOriginal ValueComments
Haze 75 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 °C
Middle Barrel Temperature 165 °C
Front Barrel Temperature 160 °C
Die Temperature 165 °CDie zone settings
Drying Temperature 80.0 °C4 hours
Moisture Content 0.080 - 0.15 %
Casting Temperature 50.0 - 60.0 °Ccasting roll for film
 
Descriptive Properties
Equipment recommendation: Screw Designcompression ration < 3low-shear design
Extruder Barrel SettingReverse temperature profile

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Telles Mirel™ A5004 Agricultural Film Grade PHA Bioplastic
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
Telles M-vera™ B5008 Film Grade Compostable Bioplastic
Telles M-vera™ B5002 Film Grade PHA Bioplastic
Telles M-vera™ B5010 Film Grade Compostable Bioplastic

PMETAA995 / 130330

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.