MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ COLORCOMP™ Compound 9X99415 Thermoplastic Polyester Elastomer (TPEE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: LNP COLORCOMP 9X99415 compound is based on Polyether Block Amide resin.

Features: Aesthetics and Appearance,Custom Color

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 0.70 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 1.10 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.015 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ISO 868
Tensile Strength, Yield 22.0 MPa50 mm/min; ISO 527
Elongation at Break >= 50 %50 mm/min; ISO 527
Elongation at Yield 20 %50 mm/min; ISO 527
Tensile Modulus 390 MPa1 mm/min; ISO 527
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 120 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 164 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 172 °CISO 11357-3
 260 °CInjection Molding
Mold Temperature 164 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80515 / 288462

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.