Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers. Availability: Latin America, North America and South America Additive: - Antiblock: 2500 ppm
- Slip: 800 ppm
- Thermal Stabilizer: Yes
Applications: - Carpet Backing
- Coextrusion Films
- Foams
- Form Fill and Seal Packaging
- Freezer Film
- High Clarity Film
- Lamination Film
Information provided by ExxonMobil |