MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Armeen T Tallow amine
Categories: Other Engineering Material

Material Notes: Armeen T is a tallow amine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.791 g/cc
@Temperature 70.0 °C
 0.799 g/cc
@Temperature 60.0 °C
 0.814 g/cc
@Temperature 38.0 °C
Viscosity 37.8 cP
@Temperature 75.0 °C
 38.8 cP
@Temperature 65.0 °C
 40.6 cP
@Temperature 55.0 °C
 44.4 cP
@Temperature 45.0 °C
Vapor Pressure 0.000133322 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.490 BTU/lb-°F
@Temperature 25.0 - 30.0 °C
 0.520 BTU/lb-°F
@Temperature 37.2 - 42.2 °C
 0.540 BTU/lb-°F
@Temperature 45.0 - 48.9 °C
Melting Point 40.0 °C
Boiling Point 260 - 350 °C
@Pressure 0.101325 MPa
Pour Point 35.0 °C
Flash Point >= 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.00 - 3.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %
 
Descriptive Properties
Amine number209-217 mg KOH/g
AppearanceSolid
Cloud point43°C
Content=5%(Mw=507), Secondary + Tertiary Amine
 =95%(Mw=262), Primary Amine
 40-60 g I2/100 gIodine value
Equivalent mass267 g/eq
HLB8.2Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY219 / 285742

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.