MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® IP 4725P Dense Extrusion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4725P is a low viscosity semicrystalline grade which offers ease of processing, fast cure rates and high states of cure with standard sulfur cure systems. It is designed for molded and extruded applications requiring low viscosity, high green strength and high finished hardness. It is ideally suited for high hardness extruded profiles and molded goods. It can also be peroxide cured.

Information provided by manufacturer.

Key Words: 0640-03-09
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.194 g/cc
Mooney Viscosity 24
@Temperature 100 °C
ML 1 + 4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 8.00 MPaVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 434 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00310 GPa
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00720 GPa
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 35.9 kN/mDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 95 %
@Temperature 125 °C
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -21.0 °CTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5TeTDC
 0.8TMTD
 1MBT
 1MBTS
 1Stearic Acid
 1.5Sulfur
 100Nordel® IP 4725P
 100N-650 Black
 100N-762 Black
 115Paraffinic Oil
 2ZnDBC
 5Zinc Oxide
 8Calcium Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 4520 Molded Golf Grip
Dow Nordel® IP 5565 General Purpose Molding
Dow Nordel® IP 4520 Molded Brake Part
Dow Nordel® IP 4520 General Purpose Molding
Dow Nordel® IP 4520 General Purpose Compound

PDVG27 / 34147

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.