MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röchling Glastic Laminates/Shapes 1580 Polyester Laminate
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS

Material Notes: Data provided by Glastic Corporation.

NEMA GPO-3. Developed to meet the television industry's safety assurance requirements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.83 g/ccASTM D792
Water Absorption 0.20 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 58.0 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Strength 170 MPaASTM D790
Compressive Strength 215 MPaASTM D695
Shear Strength 83.0 MPaASTM D732
Izod Impact, Notched 4.80 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 8.23e+14 ohmInsulation Resistance, ASTM D257
Dielectric Constant 4.0
@Frequency 1e+6 Hz
ASTM D150
 4.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmPerpendicular, Short-term, in air; ASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
ASTM D150
 0.011
@Frequency 60 Hz
ASTM D150
Arc Resistance 181 secASTM D495
Comparative Tracking Index >= 500 VUL746A
Hot Wire Ignition, HWI >= 120 secUL746A
High Amp Arc Ignition, HAI 200 arcsUL746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/minUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.270 W/m-KASTM C177
Maximum Service Temperature, Air 130 °CNEMA temperature
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 140 °CUL 746B
Flammability, UL94 V-0
Oxygen Index 39 %ASTM D2862

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
Jushi E7 DR-386T Direct Roving - Polyester Composite
Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate
Röchling Glastic T-160 Fiberglass-Reinforced Polyester Laminate

PGLASD / 41914

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.