Type of Product: Water-based adhesive. Product Characteristics: - clean machining
- fast speed of set
- easy clean-up
Typical Applications: Laminating.Suitable Substrates: Treated polyethylene and polypropylene film to paper. Information provided by H.B. Fuller Company |