MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin V0150B Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ V0150B resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. exhibits good low temperature impact resistance, damp heat performance, low moisture absorption and good dimensional stability. NORYL V0150B resin is an excellent candidate for parts that are exposed to tough outdoor environments, such as Solar / Photovoltaic (PV) junction boxes and outdoor housings and enclosures.

Features: High Heat Resistance,Non-Halogenated,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.18 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 113 MPaH358/30; ISO 2039-1
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
 60.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 70.0 MPa50 mm/min; ASTM D638
 70.0 MPa50 mm/min; ISO 527
Elongation at Break 7.0 %50 mm/min; ASTM D638
 10 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2500 MPa5 mm/min; ASTM D638
 2500 MPa1 mm/min; ISO 527
Flexural Strength 105 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 110 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2400 MPa2 mm/min; ISO 178
 2550 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 330 JASTM D256
 180 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 14.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 35CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.8
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 33.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0030
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 VIEC 60112
 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.800 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.800 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.270 W/m-KISO 8302
Hot Ball Pressure Test 140 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 130 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 135 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ISO 306
 155 °CRate B/50; ASTM D1525
 155 °CRate B/120; ISO 306
 160 °CRate A/50; ISO 306
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 115 °CUL 746B
Flammability, UL94 V-1
@Thickness >=0.800 mm
UL 94
 V-0
@Thickness >=1.00 mm
UL 94
 5VA
@Thickness >=2.00 mm
UL 94
Oxygen Index 32 %ISO 4589
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
IEC 60695-2-13
 775 °C
@Thickness 2.00 mm
IEC 60695-2-13
 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 300 °C
Zone 2 280 - 300 °C
Zone 3 300 - 320 °C
Melt Temperature 300 - 320 °CInjection Molding
Mold Temperature 100 - 130 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 80.0 - 100 °CHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82478 / 290425

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.