MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Verdant Specialty Solutions MIRATAINE® BET C-30 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Coconut oil derived amphoteric surfactant with good foaming/foam boosting properties. Economical betaine that is compatible with all surfactant classes. Irritation mollifying agent.

Chemical Name: COCAMIDOPROPYL BETAINE

CAS: 70851-07-9; 56-81-5

Available in: Asia Pacific, Europe, Latin America and North America

Compatibility: All Surfactant Classes

Use level: 1-10%

Applications: MIRATAINE® BET C-30 is an economical grade of Cocamidopropyl Betaine that is universally used in diverse personal care applications. Derived from coconut oil, MIRATAINE® BET C-30 is commonly used as a secondary surfactant in shampoos, skin cleansers, and bath products to help improve foam quality and thicken formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay. Verdant Specialty Solutions was created through the purchase of Solvay's amphoteric and secondary surfactants business

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 34 - 37 %Moisture Balance; RP-0536
pH 6.0 - 7.0RP-0420
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClean, Clear LiquidRP-0064
Color<125APHA, RP-0134
CompositionActive29-32%, Solids-Sodium Chloride
 Sodium Chloride<5.25%, RP-0097

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD281 / 137512

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.