MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sinvicomp SZF5009C Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Sinvicomp SZF5009C is a wire & cable polyvinylchloride compound available in pellet form. It provides good performance for jacketing of cables.

Availability: Asia Pacific

Uses: Wire Jacketing

RoHS Compliant:RoHS Compliant

Wire Types (IEC 60502): ST1; ST2

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccASTM D792
Deformation 25 %
@Temperature 120 °C,
Time 3600 sec
BS 6469
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Tensile Strength, Yield 2180 psiIEC 60811-1-1
 2400 psi
@Treatment Temp. 100 °C,
Time 605000 sec
Change after Aging in Air Oven; IEC 811-1-2
Elongation at Break 250 %IEC 69811-1-1
 288 %
@Treatment Temp. 100 °C,
Time 605000 sec
Change after Aging in Air Oven; IEC 811-1-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmBS 2782
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 3.20 °FASTM D746
Oxygen Index 32 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 175 °CCompression zone
 170 - 185 °CMixing zone
Feed Temperature 160 °C
Nozzle Temperature 180 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1587 / 238078

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.