MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC GELOY™ HRA222 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA flame retardant, excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Water Absorption 0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmSABIC method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
 51.0 MPa5 mm/min; ISO 527
 56.0 MPa50 mm/min; ASTM D638
 66.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 59.0 MPa5 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
 62.0 MPa5 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 50 %50mm/min; ISO 527
 >= 50 %5 mm/min; ISO 527
 >= 100 %50mm/min; ASTM D638
 >= 100 %5 mm/min; ASTM D638
Elongation at Yield 4.2 %5 mm/min; ASTM D638
 4.3 %5 mm/min; ISO 527
 4.3 %50 mm/min; ASTM D638
 4.4 %50 mm/min; ISO 527
Tensile Modulus 2520 MPa1mm/min; ISO 527
 2590 MPa5 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa2 mm/min; ISO 178
Flexural Modulus 2510 MPa2 mm/min; ISO 178
Izod Impact, Notched 385 J/mASTM D256
 290 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 69.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 71.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 102 °CRate B/50; ISO 306
 104 °CRate B/120; ISO 306
 111 °CRate A/50; ISO 306
Flammability, UL94 V-2
@Thickness 0.800 mm
UL 94
 V-0
@Thickness 2.00 mm
UL 94
 5VB
@Thickness 2.30 mm
UL 94 by SABIC-IP
 5VB
@Thickness 2.30 mm
UL 94
Oxygen Index 29 %ISO 4589
Glow Wire Test 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 220 - 260 °CInjection Molding
Zone 1 200 - 230 °C
Zone 2 220 - 260 °C
Zone 3 230 - 270 °C
Melt Temperature 230 - 270 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10142 / 243609

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.