MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® EF02 Epoxy Curing System after THR 120 EF01 S50 37% Curing Cycle  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Flexural Yield Strength 185.78 ksi
@Temperature 50.0 °C
Flexure Long; 30 min @ 250°F; prEN 2563
 200.29 ksi
@Temperature 50.0 °C
Flexure Long; 15 min @ 250°F; prEN 2563
 222.06 ksi
@Temperature 22.8 °C
Flexure Long; 15 min @ 250°F; prEN 2563
 233.67 ksi
@Temperature 22.8 °C
Flexure Long; 30 min @ 250°F; prEN 2563
Flexural Modulus 13210 ksi
@Temperature 50.0 °C
Flexure Long; 30 min @ 250°F; prEN 2563
 13500 ksi
@Temperature 22.8 °C
Flexure Long; 15 min @ 250°F; prEN 2563
 13500 ksi
@Temperature 22.8 °C
Flexure Long; 30 min @ 250°F; prEN 2563
 13500 ksi
@Temperature 50.0 °C
Flexure Long; 15 min @ 250°F; prEN 2563
Shear Strength 8.27 ksi
@Temperature 50.0 °C
ILSS Weft; 30 min @ 250°F
 8.71 ksi
@Temperature 50.0 °C
ILSS Weft; 15 min @ 250°F
 11.32 ksi
@Temperature 22.8 °C
ILSS Long; 30 min @ 250°F
 11.61 ksi
@Temperature 22.8 °C
ILSS Long; 15 min @ 250°F
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature -17.7 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXC072 / 98542

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.