MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
Categories: Polymer; Thermoset

Material Notes: The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance and excellent passive intermodulation response required for mobile infrastructure microstrip antenna applications.

Features:

  • Loss range (0.0020 to 0.0037)
  • Dk range (3.3 to 3.5)
  • Low PIM response
  • Thermoset resin system
  • Excellent dimensional stability
  • Uniform mechanical properties
  • High thermal conductivity
  • Lead-free process compatible

Benefits:

  • Wide range of application use, including Cellular infrastructure base station antennas and WiMAX antenna networks
  • Compatible with standard PCB fabrication
  • Greater yield on larger panel sizes
  • Robust handling and long life in use with thin materials
  • Improved power handling

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccASTM D792
Moisture Absorption at Equilibrium 0.020 %D48/50; IPC-TM-650 2.6.2.1; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 7.00 pliCopper; 1 oz. EDC post Solder Float; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.22 - 3.38
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
Dielectric Strength >= 500 V/mil
@Thickness 0.510 mm
Z Direction; IPC-TM-650 2.5.6.2
Dissipation Factor 0.0020
@Frequency 2.50e+9 Hz
Z direction; IPC-TM-650 2.5.5.5
 0.0025
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature -55.0 - 288 °C
Y-Direction; ASTM D3386-94
 13.0 µm/m-°C
@Temperature -55.0 - 288 °C
X-Direction; ASTM D3386-94
 37.0 µm/m-°C
@Temperature -55.0 - 288 °C
Z-Direction; ASTM D3386-94
Thermal Conductivity 0.600 W/m-K
@Temperature 80.0 °C
ASTM C518
Glass Transition Temp, Tg >= 280 °CTGA, Condition A; IPC-TM-650 2.4.24
 
Descriptive Properties
Dimensional Stability< 0.2 mm/mX, Y directions; after etch; IPC-TM-650, 2.4.39A
PIM150 - 160 DbcSummitek 1900b PIM analyzer; Reflected 43 dBm swept tones

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate

PROGA958 / 138398

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.