MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1652 M (SEBS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1652 M is a translucent, linear triblock copolymer based on styrene and ethylene/butylene (SEBS) with a Styrene / Rubber ratio of 30/70. It is supplied from North America in the physical form identified:
Kraton G1652 MU - supplied as an undusted powder
Kraton G1652 MS - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1652 M is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Bitumen Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D4025
Volatiles <= 0.60 %KM 04
Viscosity 400 - 525 cP20% Toluene Solution at 25°C; BAM 922
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 69
@Time 10.0 sec
ASTM D2240
Tensile Strength 31.0 MPaASTM D412
Elongation at Break 500 %ASTM D412
300% Modulus 0.00483 GPa
@Strain 300 %
ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.1%, KM 08
 Polystyrene29-30.8%, Measured on the polymer before hydrogenation, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio30/70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1161 P (SIS) Linear Triblock Copolymer
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G1701 M (SEP) Linear Diblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer

PKRA9896 / 132795

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.