Anaerobic GasketingLoctite® 5205 Flexible Cure Flange Sealant Fast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recommended Primer: 7649 (N) or 7471 (T). Typical Use: Fast curing, flexible |