MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FR-P38 Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD is the largest manufacturer of flame retardant in Taiwan. We have nearly 40 years of experience developing functional additives and providing a series of solutions for general plastic and engineering plastic industry.

Applications:

  • Various PU foam and foaming fireproof application
  • Rubber industries: a variety of natural and synthetic rubber, including SBR.NBR.CR
  • PVC product ( film/ synthetic leather/ cable)
  • PU Synthetic Leather fireproof application
  • PC/ABS alloy and engineering plastic
  • Coating
  • All kinds of thermal setting resin and thermal plasitc
  • Phenolic resin, cellulose resin, epoxy resin, Polyurethane Resin polyvinyl acetate (PVB). nitrocellulose(CN). Acetate cellulose (EC)
  • Phenolic and epoxy copper claded laminates
  • Various flexible and rigid Printed circuit board fireproof application
Advantages:
  • Provide excellent flame retard effect
  • With good fireproof stability
  • Confer PU foam product outstanding flame retardability
  • Remarkable electric insulativity
  • Outstanding hydrolysis resistance effect
  • Good oil resistance
  • Low temperature resistance ( also in room temperature with good flexibility )
  • Good compatibility with resin?PVC?PU?PMMA?PS
  • Excellent wear resistance

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.205 - 1.215 g/cc
Viscosity 30 - 50 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050mg KOH/g
 
Thermal PropertiesOriginal ValueComments
Boiling Point 245 °C
@Pressure 0.000530 MPa
 
Descriptive Properties
Appearanceliquid
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN073 / 266381

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.