PREBLACK PE 700-40 is a polyethylene based black masterbatch. PREBLACK PE 700-40 has been developed for the coloring of PE-LD and PE-HD products when maximum UV-resistance and pureness is being required. The moisture absorption and sulphur content of PREBLACK PE 700-40 are very low preventing odor problems. According to BgVV regulations PREBLACK PE 700-40 is approved for use in contact with foodstuffs as long as the content of carbon black in the produced product is less than 2.5%. Information provided by Premix Thermoplastics Inc. |