MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound MFD02 Polypropylene, Unspecified (PP, Unspecified)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP STAT-KON MFD02 compound is based on Polypropylene (PP) resin containing conductive carbon powder and 10% glass fiber. Added features of this grade include: Electrically Conductive.

Features: Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
 1.05 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm24hrs; ASTM D955
 0.012 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.011 - 0.013 cm/cm24hrs; ASTM D955
 0.012 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPaASTM D638
 23.0 MPaISO 527
Tensile Strength, Yield 28.0 MPaASTM D638
 28.0 MPaISO 527
Elongation at Break 4.1 %ISO 527
 6.1 %ASTM D638
Elongation at Yield 2.9 %ISO 527
 3.2 %ASTM D638
Tensile Modulus 2430 MPa1 mm/min; ISO 527
 2750 MPa50 mm/min; ASTM D638
Flexural Strength 43.0 MPaISO 178
Flexural Modulus 2060 MPaASTM D790
 2200 MPaISO 178
Izod Impact Notched 133 JASTM D256
Izod Impact, Unnotched 379 J/mASTM D4812
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 16.0 Jpeak; ASTM D3763
Impact Test 11.0 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 10 - 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 64.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 103 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 103 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 127 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 133 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 85.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 240 - 250 °C
Melt Temperature 225 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81322 / 289269

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.