MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexForce™ 3784 Fiber Glass Fabric
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 24.2 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Impact 925 ft-lb/inFilling Breaking Strength
 1150 ft-lb/inWarp Breaking Strength
 
Descriptive Properties
Fabric Weight (oz/yd2)25.79Dry
Nominal Construction (count/in)36Fill
 45Warp
Type of YarnFill Yarn: ECG 37 1/2
 Warp Yarn: ECG 37 1/2
Weave Style8 Harness Satin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo Zylon® HM Poly(p-phenylene-2,6-benzobisoxazole) Fiber
Toyobo Zylon® AS Poly(p-phenylene-2,6-benzobisoxazole) Fiber
Norplex-Micarta NorPLY™ 1002 Epoxy Fiberglass Composite, Unidirectional
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric
Hexcel® HexForce™ 112 Fiber Glass Fabric

PHEXC611 / 101230

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.