MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crosspolimeri EFRHATAN 702 Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Efrhatan: is the trade-mark of our modified polyurethane (PUR)

Efrhatan 702: copolymer TPU (ether base) for technical sheathing extrusion

Certify: H07BQ-F COMPRESSION EXTRUSION

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccISO 1183
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87ISO 868
Tensile Strength 35.0 MPaISO 527
 45.5 MPa
@Temperature 120 °C,
Time 605000 sec
Heat Ageing; UL 1581
 45.5 MPa
@Temperature 121 °C,
Time 64800 sec
Ageing in oil ASTM II; UL 1581
Elongation at Break 540 %ISO 527
 702 %
@Temperature 120 °C,
Time 605000 sec
Heat Ageing; UL 1581
 702 %
@Temperature 121 °C,
Time 64800 sec
Ageing in oil ASTM II; UL 1581
Tear Strength 75.0 kN/mambient; DIN 53515
Abrasion 35[mm³]; DIN 53516
 
Processing PropertiesOriginal ValueComments
Zone 1 165 °C
Zone 2 175 °C
Zone 3 185 °C
Zone 4 190 °C
Die Temperature 215 - 225 °C
Head Temperature 195 °C
Dry Time 3.00 hour
@Temperature 100 °C
 6.00 hour
@Temperature 100 °C
 
Descriptive Properties
Cold Flex-40°CISO 458
Exercise temperature90°C
Saponification Resistance<200 Mg KOH/gHD 22.10S1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS023 / 294107

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.