ALATHON H5623X01 provides easy processing characteristics and exhibits excellent toughness properties, color and good processing stability. Typical applications include housewares, containers, caps and closures. Regulatory Status: H5623X01 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing H5623X01 can only be made when the processing conditions, equipment and end use application are known. This product is from the former Equistar product line. |