MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 provides excellent chemical resistance with minimal particle generation. Available in a wide range of geometries and cross sections, this material offers the diversity required for a variety of dynamic or static dry processing applications.

Applications:

  • Door seals
  • Slit valves
  • Window seals
  • Isolator valve seals
  • Lid seals
  • Gas inlet seals
  • KF fitting seals
  • Chamber seals
  • Valve seals
  • Endpoint windows

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.11 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82ASTM D2240
Tensile Strength at Break 1870 psiASTM D1414
Tensile Strength, Yield 600 psi@50% Elongation; ASTM D1414
 1040 psi@100% Elongation; ASTM D1414
Elongation at Break 190 %ASTM D1414
Compression Set 15 %
@Temperature 204 °C,
Time 252000 sec
At 25% deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 600 °F
Minimum Service Temperature, Air -4.00 °F
 
Descriptive Properties
ColorOff-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Sandvik Osprey SAE 52100 (100Cr6) Low Alloy Steel Powder
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round

PGREEN31 / 42325

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.