MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 1458 Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly 1458 is a self-extinguishing and self-adhesive modified epoxy resin system for monolithic and sandwich structures. HexPly 1458 has excellent temperature and moisture resistance. It has a versatile cure cycle at 160°C to 180°C and it has an excellent shelf life at room temperature. HexPly 1458 prepregs are only available in fabric form.

Benefits and Features:

  • Self extinguishing.
  • Self adhesive on honeycomb and foam.
  • Controlled flow matrix.
  • Excellent tack life.
  • Suitable for a range of pressure (0.8 to 5 bar).
  • Versatile cure regime 160 - 180°C.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccCured resin
Viscosity 6000 cP
@Temperature 135 °C
 20000 cP
@Temperature 150 °C
 100000 cP
@Temperature 152 °C
 200000 cP
@Temperature 85.0 °C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 145 - 155 °CDMA
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 180 °C
at a pressure between 0.8 and 5 bar
 3.00 hour
@Temperature 160 °C
at a pressure between 0.8 and 5 bar
Gel Time 1.00 min
@Temperature 180 °C
 10.0 min
@Temperature 140 °C
 20.0 min
@Temperature 125 °C
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9117 / 322273

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.