MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake LF2020AA LLDPE, Hexene Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: LF 2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include stretch films, heavy duty bags and sacks, agricultural films, and trash bags & liners. This Kosher compliant material is available with various slip and antiblock levels. Test specimens for blown film: nominal thickness 1.0 mils fabricated at 420 F, 2.5:1 BUR, with 100 mil die gap. This product has some 21 CFR clearances. Application/Uses: Bags and sacks- Agricultural films- Trash bags and liners- Co-extruded structures.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Thickness 1.00 milBlown Film as Tested
Melt Index of Compound 1.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 670 %ASTM D882
Film Elongation at Break, TD 900 %ASTM D882
Elmendorf Tear Strength, MD 300 g/mil
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength, TD 700 g/mil
@Thickness 0.0254 mm
ASTM D1922
Dart Drop 220 g/mil
@Thickness 0.0254 mm
ASTM D1709
Dart Drop Test 220 g
@Thickness 0.0254 mm
ASTM D1709
Film Tensile Strength at Break, MD 5900 psiASTM D882
Film Tensile Strength at Break, TD 4100 psiASTM D882
1% Secant Modulus, MD 30000 psiASTM D882
1% Secant Modulus, TD 36000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 15 %no antiblock; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 410 - 440 °Fblown fim extrusion
Die Opening 0.100 inBlown Film as Tested
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWESF8829 / 222901

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.