MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ITW Devcon® Floor Patch™ FC
Categories: Polymer; Thermoset

Material Notes: A fast-curing, concrete patching compound that bonds to concrete, brick, masonry, metal, or wood and returns repair area to service in three hours. Uses: Fast curing repairs to concrete floors where medium to heavy traffic on the floor in 3 hours is needed. Used to repair expansion joints which have been damaged by forklift traffic. Used to anchor metal rails in concrete. Features: Bonds to damp surfaces, Easily troweled to 1/4" or more, Applies on cold or damp surfaces (with primer).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Compressive Strength 8000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 90.0 °FApplication Temperature
Cure Time 1.00 hour
@Temperature 29.0 °C
Functional cure
 3.00 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 15.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Aggregate/Liquid Ratio3:1By volume
 4.47:1By weight
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Chlorinated Solvent: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayCured
Coverage4.5 ft²Cured. @ 1/4"
Mix Ratio by weight2:1
Recoat Time1 hr
ViscosityPutty-paste. Mixed.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9212 / 239721

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.