MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Greene Tweed AR™ HT Abrasive-Resistant Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outstanding chemical, thermal shock and impact resistance, making it a better wear material than traditional rubber, ceramic or bronze materials.

Greene Tweed’s proprietary AR thermoplastic materials exhibit outstanding wear characteristics in media containing solids. AR combines excellent abrasive resistance, good dry run capability and superior vibration dampening characteristics with no hydrolysis or swell.

ARHT works well in a variety of abrasive pump applications iuncluding those working with sirculatiing water, open and closed cooling water, river water, screen wash and crude oil pumps. When using ARHT pump users can operate their equipment with much tighter clearances, boosting efficiency and improving process reliability.

Applications:

  • Circulating water pumps
  • Crude oil multistage pumps
  • Open and closed cooling water pumps
  • River water pumps
  • Screen wash pumps
  • Sump pumps

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.63 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Tensile Strength, Yield 5100 psiASTM D638
Elongation at Break 2.2 %ASTM D1457
Tensile Modulus 461000 psiASTM D638
Flexural Strength 8700 psiASTM D790
Flexural Modulus 495000 psi
@Strain 0.5 %
Secant; ASTM D790
Compressive Strength 9800 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µin/in-°F
@Temperature 100 °C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed Avalon® 44 PTFE, Mineral, Molybdenum Filled
Greene Tweed AR™ 1 Abrasive-Resistant Thermoplastic
Greene Tweed Arlon® 2000 Polyketone
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Greene Tweed Arlon® 1330 PEEK

PGREEN70 / 42364

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.