MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Solvay DURAPHOS® DBHP Dibutyl hydrogen phosphite
Categories: Fluid

Material Notes: Chemical Name: Dibutyl Hydrogen Phosphite

CAS: 1809-19-4

Available in: Asia Pacific, Europe, Latin America and North America

Chemical Formula: C8H19PO3

Applications: DURAPHOS DBHP (Dibutyl Hydrogen Phosphite) can be used as an intermediate in the formation of extreme pressure (EP), antiwear (AW) and friction modifier (FM) additives in lubricating oils and greases.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 - 0.990 g/ccRPC11002
Viscosity 2.0 - 3.0 cP
Molecular Weight 194.2 g/mol
Vapor Pressure 7.00 torr
@Temperature 118 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 3.5[mg KOH/g]; RPC11017
 
Thermal PropertiesOriginal ValueComments
Boiling Point 118 - 119 °C
@Pressure 0.000912 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.422 - 1.424RPC11003
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear Liquid
Color<50APHA, RPC11004
CompositionDBHP By A/B Titration>94.5%, RPC91108
 DBHP BY GC>95%, RPC91101
 Phosphorus15.5-16%, RPC91111
Turbidity<10 NTURPC11005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD300 / 137531

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.