MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Baytec® ENC-190P Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec ENC-190P is a 2,000-molecular-weight polypropylene oxide-based diol.

Properties / Applications: Baytec ENC-190P is a 2,000-molecular-weight polypropylene oxide-based diol. This diol is typically used as a flexibilizer in combination with other polyols, Baytec ENC-88 isocyanate, and Baylith® T or L Paste to produce cured polyurethanes for cable joint-sealing applications. As with any product, use of Baytec ENC-190P polyol in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
Bulk Density 62.7 lb/ft³
Viscosity <= 400 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.020[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 216 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.030 %
 
Descriptive Properties
AppearanceClear viscous liquid
Color<50APHA
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0242 / 202025

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.