MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epsan Eplamid HT00 GFR 60 NC Q1H001 Copolyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Partially aromatic copolyamide with a combination of semi-crystalline polyamide reinforced with 60% glass fiber, heat stabilized and lubricated for injection molding process.

Eplamid HT00 grades offer the following unique properties in general conditions, and even after moisture absorption:

  • Good surface finish
  • Good dimensional stability
  • Good high temperature properties
  • Outstanding chemical resistance to glycols and oils
  • Excellent creep resistance

Eplamid HT00 grades are used for molding technical parts where higher operating temperatures and higher stiffness in moist environments are required.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/ccISO 1183
Moisture Absorption 1.10 %ISO 62
Linear Mold Shrinkage, Transverse 0.0010 cm/cmISO 294
 0.0030 cm/cmISO 294
Ash 60 %ISO 3451-4
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 355 MPaConditioned; ISO 2039-1
 360 MPaDry; ISO 2039-1
Tensile Stress 255 MPaConditioned; ISO 527
 265 MPaDry; ISO 527
Elongation at Break 1.5 %Dry; ISO 527
 1.5 %Conditioned; ISO 527
Tensile Modulus 21500 MPaConditioned; ISO 527
 22000 MPaDry; ISO 527
Charpy Impact Unnotched 90.0 kJ/m²Dry; ISO 179/2-1eU
 90.0 kJ/m²Conditioned; ISO 179/2-1eU
 90.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/2-1eU
 90.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/2-1eU
Charpy Impact, Notched 13.0 kJ/m²Dry; ISO 179/2-1eA
 13.0 kJ/m²Conditioned; ISO 179/2-1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/2-1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/2-1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mmDry; IEC 60243-1
 35.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VEN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 315 °CISO 11357
Maximum Service Temperature, Air 140 °CLong Term; ISO 2578
 250 °CShort Term; ISO 2578
Deflection Temperature at 1.8 MPa (264 psi) 285 °CISO 75
Deflection Temperature at 8.0 MPa 220 °CISO 75
Flammability, UL94 HB
@Thickness 0.800 mm
ISO 1210

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LV-5H PA12-GF50
DuPont Mobility and Materials Crastin® SK615SF NC010 PBT-GF30
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry
Celanese Zytel® HTN52G35HSL BK083 PA6T/66-GF35
Celanese VECTRA MT1345 LCP, 30% Medical Technology

PEPSAN117 / 186431

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.