MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® 3200 Polyethersulfone (PESU), Transparent
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Transparent, FDA compliant, low melt flow for extrusion and injection molding

Veradel® 3200 is a low melt flow general purpose amorphous PESU resin for extrusion and injection molding. This transparent grade offers high heat deflection temperature, excellent toughness and dimensional stability and resistance to mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. Veradel® 3200 is FDA compliant and is approved for direct food contact. This grade was formerly marketed as Gafone™ PESU.

Applications: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Microwave Cookware

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; General Purpose; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium Rigidity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cmASTM D955
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 88.9 MPaASTM D638
Elongation at Yield 6.5 %ASTM D638
Tensile Modulus 2690 MPaASTM D638
Flexural Strength 125 MPaASTM D790
Flexural Modulus 2620 MPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.70e+15 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
 3.51
@Frequency 60 Hz
ASTM D150
 3.54
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mmASTM D149
Dissipation Factor 0.0017
@Frequency 60 Hz
ASTM D150
 0.0022
@Frequency 1000 Hz
ASTM D150
 0.0056
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 200 °CAnnealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Zone 1 335 - 391 °CExtrusion
Zone 2 335 - 391 °CExtrusion
Zone 3 335 - 391 °CExtrusion
Zone 4 335 - 391 °CExtrusion
Zone 5 335 - 391 °CExtrusion
Adapter Temperature 327 - 371 °CExtrusion
Die Temperature 327 - 371 °CExtrusion
Melt Temperature 343 - 385 °CInjection
 343 - 391 °CExtrusion
Mold Temperature 149 - 163 °C
Drying Temperature 177 °C
@Time 9000 sec
 177 °C
@Time 9000 sec
Extrusion
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsPowder
Injection RateFast
ProcessingCompounding; Extrusion; Injection Molding
Screw Compression Ratio2.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4588 / 280388

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.