MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Milube® Grease 2100 NLGI No. 1
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic of the steel, aluminum and rubber manufacturing industries. Excellent for use in systems requiring heavy base oil for lubrication where grease pumpability is a concern, such as industrial centralized lube systems. Milube Grease 2100T is identical to Milube 2100 with the addition of an effective tackifier. This helps the grease stay in place under high-temperature or heavily loaded conditions.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 64Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 1946 SUSBase Oil Property
Saybolt Viscosity at 210°F 113 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 420 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 23.4 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 45
Four Ball Extreme Pressure, Weld Load 400 kg
Four Ball Wear 0.500 mm
Penetration P(60), 1/10 mm 320
Timken Test 50.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 265 °F
Minimum Service Temperature, Air 5.00 °F
Pour Point 10.0 °F(Base Oil Property)
Dropping Point 450 °F
 
Descriptive Properties
ASTM Rust A&BPass
ColorBlack
Copper Corrosion2C
Low Temperature Mobility0.1 gm/secat 0°F
 0.2 gm/secat 10°F
 0.4 gm/secat 20°F
Roll Stability3% Change
Soap Type (Thickener)Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON212 / 75249

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.