MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax CA 721 GW Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax CA 721 GW is a flexible polypropylene resin used for waterproofing applications. It is manufactured using the LyondellBasell’ s proprietary Catalloy process technology. Hifax CA 721 GW membranes can be produced on slot die extruders, circular die (Blown film) extruders and on most of the calendering units.

 Hifax CA 721 GW is available in natural pellet form, and is UV light stabilized. Example uses of Hifax CA 721 GW are to produce flexible membrane, fish pond liner, snow lagoon membrane, tunnel lining, water reservoir liner, floating cover, soil and waste sheet and flexible profiles. Hifax CA 721 GW is not intended for medical and pharmaceutical applications. Applications: Geomembranes, Soft Profile & Sheets, Soil & Waste Sheet, Waterproofing Liner.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccMethod A; ISO 1183-1
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30
@Time 15.0 sec
ISO 868
Tensile Strength at Break 11.0 MPaISO 527-1,-2
Elongation at Break >= 500 %ISO 527-1,-2
Flexural Modulus 90.0 MPaISO 178
Charpy Impact, Notched >= 5.00 kJ/m²
@Temperature -40.0 °C
ISO 179
 >= 110 kJ/m²
@Temperature -20.0 °C
ISO 179
 >= NB
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 60.0 °CA50; ISO 306
DSC Induction Temperature 142 °CISO 11357-3
 
Descriptive Properties
Processing MethodBlown Film, Calendaring, Extrusion Flat-die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
Chengdu Polyster KLX-G42 PC Film & Sheet
Carmel Olefins Capilene® G 70 TF Polypropylene Homopolymer

PEQT7208 / 218845

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.