MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Armacell HT Armaflex® Industrial IMO FEF Insulation
Categories: Other Engineering Material

Material Notes: Description: HT/Armaflex® Industrial IMO is a flexible, high density and mechanically robust, closed cell thermal insulation material based on extruded elastomeric foam. The product has been specially developed for industrial offshore environments which require IMO compliant solutions.

Special features: This product us resistant to elevated operating temperatures. The product is suitable for use in multi-layer applications including Aram-Sound Industrial Systems.

Application: Thermal insulation/protection of pipes, vessels and ducts (incl. elbows, fittings, flanges etc.) in offshore, industrial (typically oil & gas) and process equipment facilities. HT/Armaflex® Industrial IMO is also used as a component of Arma-Sound Industrial Systems to provide acoustic insulation on industrial pipework and vessels ensuring reduction of sound transmission.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.70 - 5.30 lb/ft³ASTM D1622
Water Absorption <= 0.10 %ASTM C209
pH 7.0 - 9.0ISO 10523
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 2.20 psi
@Strain 25 %
ISO 6916-1
Tear Strength 2.28 pliISO 34-1
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0430 W/m-K
@Temperature -50.0 °C
EN ISO 13787
 <= 0.0440 W/m-K
@Temperature 0.000 °C
EN ISO 13787
 <= 0.0490 W/m-K
@Temperature 50.0 °C
EN ISO 13787
 <= 0.0590 W/m-K
@Temperature 100 °C
EN ISO 13787
 <= 0.0650 W/m-K
@Temperature 125 °C
EN ISO 13787
Maximum Service Temperature, Air 257 °FEN 14706, EN 14707 and EN 14304
Minimum Service Temperature, Air -58.0 °FEN 14706, EN 14707 and EN 14304
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Descriptive Properties
Water Vapor Permeability<0.05 perm-inchEN 12086 and EN 13469

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell LT Armaflex® Industrial High Density Industrial Grade, FEF Insulation
Armacell Armaflex® 520 Adhesive
Armacell AP Armaflex® SA Through 1" Self-Adhering Sheet & Roll Insulation
Mitsubishi Chemical Advanced Materials Duratron® U1000 PEI Extruded Unfilled Polyetherimide (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Acetron® GP Copolymer Acetal, Porosity-Free, Unfilled, Extruded (ASTM datasheet)

PARMD162 / 186773

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.