MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Durostone® EPC 203 Reinforced Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Durostone® EPC 203 is a tissue-fiber reinforced plastic. It is characterized by good mechanical and electrical properties and meets the thermal class F.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 350 MPaParallel; ISO 527
Modulus of Elasticity 23.0 GPaPerpendicular; ISO 178
Flexural Strength 450 MPaPerpendicular; ISO 178
Compressive Strength 500 MPaPerpendicular; ISO 604
Izod Impact, Notched (ISO) 100 kJ/m²Parallel; ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 16.0 kV/mm
@Temperature 90.0 °C
Perpendicular; EC 60243
 70.0 kV/in
@Temperature 90.0 °C
Parallel; IEC 60243
Comparative Tracking Index 180 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 - 20.0 µm/m-°C
Thermal Conductivity 0.300 W/m-KISO 8302
Maximum Service Temperature, Air 155 °CThermal Endurance; TI, IEC 60216
 
Descriptive Properties
Colorgreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Solvay CYCOM® 754 Epoxy Resin with 36% - HS - 200 – 300; 75°C Cure
Röchling Glastic® EPC 205 Reinforced Epoxy Resin
Röchling Durostone® EPM 203 Reinforced Epoxy Resin

PROCH9079 / 232782

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.