ATOFINA Polypropylene PPR 3400 MA3 is a nucleated and antistatic random copolymer polypropylene for the injection molding of articles with high transparency and excellent surface appearance. Application ATOFINA Polypropylene PPR 3400 MA3 is intended for household goods and thin walled packaging. Information provided provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |