Emerson & Cuming 45C Eccobond® Two-Component General Purpose Epoxy Adhesive Clear, unfilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of Catalyst 15 used. Convenient mix ratio. Good impact resistance. Excellent adhesion to metal, glass and plastic substrates. Mix Ratio of 100:100 to 100:300 (Cat 15 CLEAR variation). Bonding Type: Epoxy The Eccobond® product line is now a part of Henkel; this specific grade is discontinued. |