EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antiblock additives. EVATANE 42-60 is readily dissolved into solvent and can be used in inks or solvent adhesives. The High Vinyl Acetate content of EVATANE 42-60 brings softness, flexibility, polarity and high solubility.Information provided by Arkema Group |