MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Si 75® Organosilane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Si 75® is a bifunctional, sulfur-containing organosilane for rubber applications in combination with white fillers containing silanol groups.

Description: Si 75® reacts with silanol groups of white fillers during mixing and with the polymer during vulcanization under formation of covalent chemical bonds. Compared to the polysulfidic organosilane Si 69®, Si 75® has a higher temperature stability and therefore allows higher mixing temperatures. Si 75® imparts greater tensile strength, higher moduli, reduced compression set, increased abrasion resistance and optimized dynamic properties.

Application fields are: Low rolling resistance tires

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccTamped; DIN 51757
Molecular Weight 486 g/mol
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 15.3 %SOP 2000-19
 
Descriptive Properties
Appearancelight yellow to brownish clear liquid
Average sulfur chain length, HPLC2.35ASTM D6844
By-products, GC<3.5%ASTM D6843

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIN007 / 317041

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.