Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples: DIN 73378: Tubes made from Polyamide for Automotive vehicles Information provided by EMS Grivory. |