MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ INP984 ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: SABIC INP 984 is a 45% polybutyl acrylate rubber grafted weatherable ASA modifier resin. Provides excellent impact, heat distortion and weatherability properties. Maintains polymer properties in UV and thermal environments. Toughens compatible rigid polymers without additional impact modification. Expands the use temperature window of compounds. Offers compatibility with many polar polymers. Improve UV resistance when blended with less stable polymers. SABIC INP984 is well suited to produce good weatherability in rigid polymer applications. Can be effectively alloyed with PVC and other miscible thermoplastics in molded, extruded or calendered applications to provide improved heat distortion

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Bulk Density 0.260 g/ccASTM D1895
Density 1.07 g/ccMolded; ISO 1183
Volatiles 0.10 %SABIC method
Particle Size 465 µmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
 
Descriptive Properties
Rubber45 %SABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10075 / 243542

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.