MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DX94375H Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DX94375H compound is based on Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Healthcare, Wear Resistant.

Features: Healthcare,Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D792
 1.27 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0090 - 0.011 cm/cm24hrs; ASTM D955
 0.0090 - 0.011 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm24hrs; ASTM D955
 0.010 - 0.012 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 43.0 MPaISO 527
 44.0 MPaASTM D638
Tensile Strength, Yield 49.0 MPaISO 527
 52.0 MPaASTM D638
Elongation at Break 52 %ISO 527
 56 %ASTM D638
Elongation at Yield 5.1 %ISO 527
 5.7 %ASTM D638
Tensile Modulus 1860 MPa50 mm/min; ASTM D638
 2100 MPa1 mm/min; ISO 527
Flexural Strength 68.0 MPaASTM D790
 81.0 MPaISO 178
Flexural Modulus 2040 MPaASTM D790
 2300 MPaISO 178
Izod Impact Notched 149 JASTM D256
Izod Impact, Notched (ISO) 19.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 137 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 33.0 Jpeak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80761 / 288708

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.