MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Edgetek® X TR2-40TA/000 NATURAL Copolyester with Mineral Filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Eastman Tritan™ copolyester these compounds provide chemical resistance, clarity, heat resistance and BPA-free solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.00010 - 0.00020 cm/cm
@Thickness 3.18 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.8 MPaType I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 53.8 MPa5.1 mm/min; ASTM D638
Elongation at Break 1.5 %Type I, 5.1 mm/min; ASTM D638
Elongation at Yield 1.5 %5.1 mm/min; ASTM D638
Tensile Modulus 7520 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa1.3 mm/min; ASTM D790
Flexural Modulus 6040 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 37.4 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Izod Impact, Unnotched 3.20 J/cm
@Thickness 3.18 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
TMA; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 108 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 266 - 282 °C
Mold Temperature 60.0 - 65.6 °C
Drying Temperature 87.8 °C
@Time 14400 sec
 
Descriptive Properties
FeaturesBPA Free
 Crazing Resistant
 Filled
 Good Chemical Resistance
 Good Crack Resistance
 Good Dimensional Stability
 Good Toughness
 Medium Clarity
 Medium Heat Resistance
FormsPellets
Generic NameCopolyester
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliance Components
 Consumer Applications
 Food Service Applications
 Household Goods
 Industrial Applications
 Transparent or Translucent Parts

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ MX731 Medical Grade Copolyester
Avient Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)
Eastman Tritan™ LX100 Copolyester
Eastman Tritan™ LX101 Copolyester
Eastman Tritan™ LX151HF Copolyester

PH1PN8067 / 101903

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.