MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cray Valley Wingtack® 86 Aromatically Modified C-5 Hydrocarbon Resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Wingtack® 86 is a light yellow aromatically modified resin that possesses an excellent balance of tack, peel and cohesive strength. It is further characterized by light color, low odor and volatility, low melt viscosity, low specific gravity, and very good viscosity and color stability at compounding temperatures.

Product Highlights / Performance Properties:

  • Compatible with a wide variety of polymers, elastomers, olefins, and waxes including SBC, SBR, SBS, SIBS, EVA, acrylics and urethanes
  • Generally soluble in solvents having low to medium polarity
Suggested Applications:
  • Hot melt adhesives (HMA)
  • Pressure sensitive adhesives (PSA)
  • Coatings & Paints
  • Roofing membrane
  • Waterproofing
  • Sealants
  • Plastics & Rubber

Information provided by Cray Valley

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D891
Molecular Weight 650 g/molMn
 1300 g/molMw
Ash 0.00 %
 
Thermal PropertiesOriginal ValueComments
Softening Point 87.0 °CE-950
Glass Transition Temp, Tg 42.0 °Cmidpoint
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 1.5in 50% toluene; E-803
 
Descriptive Properties
AppearanceLight yellow
Clarity0.97E-803a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCRAYV042 / 316195

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.