MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Xytron™ TC6022I PPS-(GF+MX)60 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.

Features: Thermal conductive. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
Hardness, Shore M 100ISO 2039-2
Tensile Strength at Break 55.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 63.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 78.5 MPa
@Temperature 120 °C
ISO 527-1/-2
 120 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Elongation at Break 0.70 %
@Temperature 23.0 °C
ISO 527-1/-2
 1.2 %
@Temperature 120 °C
ISO 527-1/-2
 1.3 %
@Temperature 180 °C
ISO 527-1/-2
 1.5 %
@Temperature 160 °C
ISO 527-1/-2
Tensile Modulus 9150 MPa
@Temperature 180 °C
ISO 527-1/-2
 9900 MPa
@Temperature 160 °C
ISO 527-1/-2
 12200 MPa
@Temperature 120 °C
ISO 527-1/-2
 22000 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Flexural Modulus 10100 MPa
@Temperature 180 °C
ISO 178
 11000 MPa
@Temperature 160 °C
ISO 178
 13800 MPa
@Temperature 120 °C
ISO 178
 23200 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact Unnotched 16.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Comparative Tracking Index 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CISO 11359-1/-2
 72.0 µm/m-°Cabove Tg; ISO 11359-1/-2
CTE, linear, Parallel to Flow 11.0 µm/m-°CISO 11359-1/-2
 12.0 µm/m-°Cabove Tg; ISO 11359-1/-2
Melting Point 280 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 265 °CISO 75-1/-2
UL RTI, Electrical 130 °C
@Thickness 0.400 mm
UL746B
Flammability, UL94 V-0
@Thickness 3.00 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7964 / 291400

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.