MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C46750, H02 Temper, Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Excellent Suitability – Soldering, Capacity for Being Hot Formed; Good Suitability – Brazing; Fair Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld, Gas Shielded Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Cold Worked

Applicable Specifications: Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Rod, Bar & Shapes – Navel Brass ASTM B21/B21M, Forgings ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.310 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 148
@Load 0.500 kg
Tensile Strength 66.0 ksi
Tensile Strength, Yield 50.0 ksi0.2% Offset
Elongation at Break 23 %
Tensile Modulus 15300 ksi
Modulus of Rigidity 5670 ksi
Poissons Ratio 0.35
Machinability 60 %
Forgeability 98 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000780 ohm-cm22.1% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.39 µin/in-°F
@Temperature 20.0 - 100 °C
 10.94 µin/in-°F
@Temperature 20.0 - 200 °C
 11.5 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.100 BTU/lb-°F
Thermal Conductivity 59.6 BTU-in/hr-ft²-°F
Melting Point 1546 - 1632 °F
Solidus 1546 °F
Liquidus 1632 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature >= 878 °F
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb 0.050 - 0.15 %
Copper, Cu 59.2 - 62.5 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.25 %
Nickel, Ni <= 0.50 %
Phosphorus, P 0.050 - 0.15 %
Tin, Sn 1.0 - 1.8 %
Zinc, Zn 34.7 - 39.7 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC46750x1 / 292048

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.