MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R633H05 Nylon, Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Vydyne R633H05 is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in black, this injection-molding grade resin is lubricated for machine feed and mold release.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccDAM; ISO 1183
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 2.3 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa50% RH; ISO 527-2
 184 MPaDAM; ISO 527-2
Elongation at Break 4.0 %DAM; ISO 527-2
 6.0 %50% RH; ISO 527-2
Tensile Modulus 8000 MPa50% RH; ISO 527-2
 10800 MPaDAM; ISO 527-2
Flexural Strength 195 MPa50% RH; ISO 178
 255 MPaDAM; ISO 178
Flexural Modulus 6800 MPa50% RH; ISO 178
 8800 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 19.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 44.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 51.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 91.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 92.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
ASTM D 495
High Voltage Arc Resistance to Ignition (HVAR) 7.0 - 15 sec
@Thickness 0.750 mm
PLC 4; UL 746
 7.0 - 15 sec
@Thickness 1.50 mm
PLC 4; UL 746
 15 - 30 sec
@Thickness 3.00 mm
PLC 3; UL 746
Comparative Tracking Index >= 250 V
@Thickness 3.00 mm
IEC 60112
 <= 399 V
@Thickness 3.00 mm
IEC 60112
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
UL 746
 >= 120 arcs
@Thickness 1.50 mm
UL 746
 >= 120 arcs
@Thickness 3.00 mm
UL 746
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
@Thickness 3.00 mm
UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 233 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 230 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 220 °CUnannealed; DAM; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.750 mm
UL 94
 HB
@Thickness 1.50 mm
UL 94
 HB
@Thickness 3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Middle Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Front Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Nozzle Temperature >= 280 °CInjection
 <= 310 °CInjection
Melt Temperature >= 285 °CInjection
 <= 305 °CInjection
Mold Temperature >= 65.0 °CInjection
 <= 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA112G35
 ASTM, D6779 PA082G35
 FED, L-P-410A
 SAE, J1639 PA1816 Z6
AppearanceBlack
FeaturesCopolymer
 Good Mold Release
 Good Surface Finish
 Heat Stabilized
 High Tensile Strength
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R633H01 Nylon, Glass Filled
Envalior Akulon® K224-G6 PA6-GF30, Conditioned, 30% Glass Filled
DuPont Mobility and Materials Zytel® FE270050 BK099 PA66-(GF+MD)30
Celanese Zytel® 73G30HSL BK416 PA6-GF30
Overview of materials for Nylon 46, Glass Fiber Reinforced

PASCE9848 / 220949

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.