MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Thermal Ceramics Firebrick SR-99 LS
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: The SR-90, SR-99, and SR-99 firebricks are premium high alumina firebricks that are capable of handling very difficult applications. These premium bricks are very dense and have excellent load bearing strength at temperatures above 3000°F (1649°C) and they provide excellent thermal shock resistance. The extremely low silica content of both products make them ideal for hydrogen atmospheres.

Features:

  • 90 and 99% alumina firebrick
  • Excellent low SiO2 contents for use in Hydrogen atmospheres
  • Excellent high temperature stability
  • Extremely high service temperature
  • Applications:

  • Sulphur recovery units
  • Incinerators
  • Secondary ammonia reformers
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 3.093 g/cc
    Deformation 0.70 %at 10 psi; 100 hours at 2640°F
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.800 ksi
    @Temperature 1430 °C
     2.00 ksi
    @Temperature 1260 °C
     4.20 ksi
    @Temperature 23.0 °C
    Compressive Strength 82.76 MPa
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 19.1 BTU-in/hr-ft²-°F
    @Temperature 1370 °C
    ASTM C201
     21.6 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    ASTM C201
     25.5 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    ASTM C201
     30.7 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    ASTM C201
     38.9 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    ASTM C201
    Maximum Service Temperature, Air 3000 °F
    Shrinkage -0.170 %
    @Temperature 1760 °C,
    Time 18000 sec
     0.60 %
    @Temperature 1760 °C,
    Time 259000 sec
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 99.5 %
    Alkalis 0.20 %
    CaO 0.20 %
    SiO2 0.10 %
     
    Descriptive Properties
    Fe2O3traces
    MgO Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
    China-Yixing Longly Refractories ASM-130 Cordierite-Mullite
    Thermal Ceramics Firebrick SR-90
    Thermal Ceramics Firebrick SR-99
    Sharadaa Ceramics 32 Insulation Bricks-ASTM

    CTHERM126 / 2446

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.