MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Calsak CS-72 General Purpose ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Product Characteristics:
  • High Impact, High Gloss
  • Injection molding grade

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ASTM D785
Tensile Strength, Yield 6100 psi
@Thickness 3.17 mm
Type I; ASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 370 ksi
@Thickness 3.17 mm
Type I; ASTM D638
Flexural Strength 10500 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 380 ksi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 7.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 185 °F
@Thickness 3.17 mm
Unannealed; ASTM D648
 202 °F
@Thickness 3.17 mm
Annealed; ASTM D648
Vicat Softening Point 106 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 455 - 480 °F
Middle Barrel Temperature 465 - 490 °F
Front Barrel Temperature 475 - 500 °F
Nozzle Temperature 475 - 500 °F
Melt Temperature 475 - 575 °F
Mold Temperature 110 - 150 °F
Drying Temperature 180 - 190 °F
@Time 7200 sec
Injection Pressure 10000 - 16000 psi
Back Pressure 0.000 - 25.0 psi
Clamp Pressure 2000 - 4000 psi
 
Descriptive Properties
Hold Pressure50 - 75% of injection pressure
Injection SpeedHigh
Screw SpeedModerate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS 3500 Natural 1050
A. Schulman Diamond ABS 2510
A. Schulman Diamond ABS 1100
A. Schulman Diamond ABS 1000
A. Schulman Diamond ABS 3501 Black 1302 Injection Molding Grade

PCALSAK8 / 104054

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.