MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XTWE480 ASA (Asia)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Anti-scratch GELOY grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Density 1.15 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 38 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.0 MPa50 mm/min; ASTM D638
 38.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa50 mm/min; ISO 527
 50.0 MPa50 mm/min; ASTM D638
Elongation at Break 21 %50 mm/min; ASTM D638
 25 %50 mm/min; ISO 527
Elongation at Yield 3.0 %50 mm/min; ASTM D638
 3.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1mm/min; ISO 527
 2470 MPa50 mm/min; ASTM D638
Flexural Yield Strength 70.0 MPa2 mm/min; ISO 178
 70.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2060 MPa1.3 mm/min, 50 mm span; ASTM D790
 2410 MPa2 mm/min; ISO 178
Izod Impact, Notched 49.0 J/mASTM D256
 27.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Dart Drop, Total Energy 6.00 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 88.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 73.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 78.0 °CRate B/50; ASTM D1525
 79.0 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Zone 1 205 - 220 °CProfile Extrusion
Zone 2 210 - 225 °CProfile Extrusion
Zone 3 215 - 225 °CProfile Extrusion
Zone 4 215 - 225 °CProfile Extrusion
Adapter Temperature 200 - 225 °CProfile Extrusion
Die Temperature 210 - 225 °CProfile Extrusion
Melt Temperature 200 - 230 °C
Drying Temperature 75.0 - 85.0 °CProfile Extrusion
Dry Time 4.00 hourProfile Extrusion
Moisture Content 0.020 %
Precipitation Temperature 50.0 - 70.0 °CCalibrator
 
Descriptive Properties
Pencil Hardness test, 1kgfFASTM D3363

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10164 / 243631

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.